No.
It should be hammered out before heat is applied.
hh.
Offset crosspeen.
ii.
jj.
If the epoxy has not thoroughly cured, the body file will clog and
gouge the surface being worked on.
kk.
The process of tinning prepares a surface for receiving and holding
ll.
A light coat of oil.
mm.
Solder composed of 30 percent tin and 70 percent lead.